Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3HG6 WIT BK20560 - (PA66+PA6T/6)-(GF+GB)30 - BASF

Material Data Center offers the following functions for Ultramid® A3HG6 WIT BK20560:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Glass fibre reinforced injection moulding grade with good resistance to hydrolysis, suited for processing by water injection technology (WIT). Applications in the automotive cooling circuit, e.g. cooling water pipes.
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 8 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
Contração após a moldagem, paralelo 0.4 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.9 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 8700 / 5300 MPa ISO 527
Tensão na ruptura 165 / 95 MPa ISO 527
Deformação na ruptura 3 / 4.9 % ISO 527
Resistência ao impacto Charpy , +23°C 55 / 85 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 50 / 50 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 6 / 8 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 5 / 5 kJ/m² ISO 179/1eA
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 230 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 250 / * °C ISO 75-1/-2
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade 1370 / - kg/m³ ISO 1183
Propriedades específicas do materialSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de viscosidade 146 / * cm³/g ISO 307, 1157, 1628
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 80 °C -
Pré-secagem - tempo 4 h -
Umidade do processamento ≤0.15 % -
Temperatura da massa 290 - 310 °C -
Temperatura do molde 80 - 90 °C -
Diagrama
Viscosidade - taxa de cisalhamento , Ultramid® A3HG6 WIT BK20560, (PA66+PA6T/6)-(GF+GB)30, BASF
Tensão de cisalhamento - taxa de cisalhamento , Ultramid® A3HG6 WIT BK20560, (PA66+PA6T/6)-(GF+GB)30, BASF
Tensão - deformação , Ultramid® A3HG6 WIT BK20560 (dry), (PA66+PA6T/6)-(GF+GB)30, BASF
Tensão - deformação , Ultramid® A3HG6 WIT BK20560 (cond.), (PA66+PA6T/6)-(GF+GB)30, BASF
Módulo secante - deformação , Ultramid® A3HG6 WIT BK20560 (dry), (PA66+PA6T/6)-(GF+GB)30, BASF
Módulo secante - deformação , Ultramid® A3HG6 WIT BK20560 (cond.), (PA66+PA6T/6)-(GF+GB)30, BASF
Módulo de tração - temperatura , Ultramid® A3HG6 WIT BK20560 (cond.), (PA66+PA6T/6)-(GF+GB)30, BASF
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos, Negro
Resistência Química
Estabilidade hidrolítica
Aplicaciones
Automóvel
Disponibilidade regional
Outras informações
Moldagem por injeção
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 290 - 310 °C
injection molding, Melt temperature, recommended: 300 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
Resistência em meio químico
Ácidos
Ácido Acético (5% em massa) (23°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com